S pin coating from dilute solution is - Rensselaer Polytechnic Institute (RPI) :: Architecture, Busi

Spin Coating of Thin and ultrathin Polymer Films Table 2. Parameters for Predicting h,Values Given in Figs. 4 and 5 Using Eqs 3-5. chloroform solutions p = 1.49 g/cm3 M, = 119.4 g/rnol p10 = 0.31 atm D,, = 0.106 cm2/s T, x,,, R: wg, and c: see Table 1 xyl